RECONDITIONING PROCEDURE EXHAUST VALVE SPINDLE
![1](/images/procedure/exhaust-valve-spindle/1.jpg)
1. Worn / burned seating area
![1](/images/procedure/exhaust-valve-spindle/2.jpg)
2. Underside disc burned
![1](/images/procedure/exhaust-valve-spindle/3.jpg)
3. Worn stem (chromed or hvof coated)
![1](/images/procedure/exhaust-valve-spindle/4.jpg)
4. Premachining disc
![1](/images/procedure/exhaust-valve-spindle/5.jpg)
5. Disc welding plasma / mig
![1](/images/procedure/exhaust-valve-spindle/6.jpg)
6. Cnc machining disc
![1](/images/procedure/exhaust-valve-spindle/7.jpg)
7. HVOF coating / chroming stem
![1](/images/procedure/exhaust-valve-spindle/8.jpg)
8. Grinding / superfinishing stem
![1](/images/procedure/exhaust-valve-spindle/9.jpg)
9. Reconditioned spindle